MER Group: Antikey ya Introduksion ed Prinsipyo na Panagkimey na Twin-Shaft Kiln
Say manunan istruktura na twin-shaft kiln et tugyopen na duaran mankakasakey ya vertical shafts (Shaft A tan Shaft B), ya say inkalapagan ya vertical ya layout et mangaala na melag a pasen. Say leksab na duaran shaft et akakonekta panamegley na sakey a kanal, tan walay reversing device ya inyan ed tagey pian nagawa so panapanaon ya pananguman na saray kimey da. Say pegley na kiln et say calcining zone, say leksab et walay discharge device, tan say tagey et walay feeding tan flue gas exhaust equipment. Say manunan desinyo to et say pakagamor na epektibon pangusar na petang diad panamegley na "alternate calcination tan waste heat recovery," ya walay thermal efficiency ya masulok ya 80%.
Say prinsipyo na pantratrabaho et nibase ed lohika na "synergy ed baetan na duaran shaft tan periodic reversal," tan say espisipikon proseso et naapag ed duaran mansasalatan a siklo (kada siklo et kaslakan ya manbayag na 8-12 minuto):
Unonan Yugto (Shaft A parad Calcination, Shaft B parad Preheating/Cooling):
Say gasolina et i-inject tan poolan ed burner diad abeban parte na Shaft A, ya mamawala na atagey a temperatura na flue gas ya 1200-1300 degree. Say atagey a temperatura na flue gas et onaagus ed tagey diad Shaft A, ya manpapasnok tan mamapainit ed limestone ya inyarum manlapud tagey, kanian kalkalnan nasumpal na limestone so decomposition reaction. Kayari to, say atagey a temperatura na flue gas et onloob ed abeban parte na Shaft B diad panamegley na mankokonektaan a kanal ed tagey na duaran shaft, ya itultuloy ton painitan so limestone ed Shaft B pian naala so unonan pakabawi na flue gas waste heat. Kaleganan to, say ambetel ya dagem et onloob manlapud tagey na Shaft B, ya onaagus ed leksab pian palemewen so calcined quicklime ed Shaft B. Say ambetel ya dagem et onsesegep ed nalilikna ya petang na quicklime tan napainit ed ambetel ya dagem, ya ipawit ed Shaft A bilang dagem na panagpoolan diad leksab a kanal, ya nagawa so komaduan pakabawi na nalilikna ya petang. Diad sampot na sayan yugtan, say kinalsin ya quicklime ed Shaft A et ompaway ed leksab, tan saray materyales ed Shaft B et sigpot lan napainit.
Komaduan Yugto (Shaft B parad Calcination, Shaft A parad Preheating/Cooling):
Say kimey na duaran shaft et nauman panamegley na reversing device. Say gasolina et i-inject tan popoolan natan manlapud abeban parte na Shaft B, tan say atagey a temperatura na flue gas et onaagus ed tagey diad Shaft B pian na-calcine iray materyales, insan onloob ed Shaft A pian na-preheat so balon inyarum ya limestone. Say ambetel ya dagem et onloloob manlapud tagey na Shaft A, tan palemewen to so pinainit ya quicklime ed Shaft A, tan say pinainit ya ambetel ya dagem et manserbin combustion air parad Shaft B. Diad panamegley na ontan ya panapanaon ya pansasaliwan, say duaran shaft et tuloytuloy ya man-cycle ed saray kimey na "calcination - preheating/cooling" pian nadampot so tuloytuloy ya produksyon. Diad interon proseso, say petang na flue gas tan say petang na quicklime et sigpot ya nabawi tan nausar, kanian nabawasan so konsumo na petang na unit product.

 

 

 