Say 800 TPD double-shaft vertical kiln EPC turnkey project ya inpundo na Gansu Haixin tan ginawa na MER Group et akasabi ed malet ya inagew-agew ya produksyon ya 920 metric tons. Saray manunan pakapatnagan et kaiba so underburning rate <5% tan kiln pressure 20kPa. Walay kaaruman ya pamalaknab na kapasidad ya anggad 1000 tonelada kada agew.